Printing and Lamination for Flexible packaging, Matalizing for Flexible packaging.
Transparent high Gloss and corona on either side for excellent mechanability and printability for Flexible packaging.
Chemical coating enhances bond strength and link addition.
PROPERTIES | TEST METHOD | UNIT | PLAIN | TREATED | ||||
---|---|---|---|---|---|---|---|---|
10μ | 12μ | 10μ | 12μ | |||||
Film Code | Internal | - | APGT - 10 CC | APGT - 12 CC | APGT - 10 CC/CT | APGT - 12 CC/CT | ||
Nominal Thickness | Internal | (μ) | 10 | 12 | 10 | 12 | ||
Yield | Internal | g/m2 | 71.4 | 59.6 | 71.4 | 59.6 | ||
Haze | ASTM D- 1003 | % | 3 | 3 | 3 | 3 | ||
|
ASTM D 882 | kgs/cm2 | 2200 2100 |
2200 2100 |
2200 2100 |
2200 2100 |
||
|
ASTM D 882 | % | 100 90 |
100 90 |
100 90 |
100 90 |
||
|
ASTM D - 1204 | % | 2.5 0.5 |
2.5 0.5 |
2.5 0.5 |
2.5 0.5 |
||
|
ASTM D - 1894 | Static/Kinetic | 0.5 0.45 |
0.5 0.45 |
0.5 0.45 |
0.5 0.45 |
||
Wetting Tension Coated Side |
ASTM D - 2578 | Dyne/cm | 56 | 56 | 56 | 56 | ||
Wetting Tension | ASTM D - 2578 | Dyne/cm | 44 | 44 | 50 | 50 | ||
WMVTR (38°C & 90% RH) typical |
ASTM D - 1249 | gm/m2/day | 40 | 40 | 40 | 40 | ||
OTR (23°C & 0% RH) typical |
ASTM D - 3985 | cc/m2/day | 130 | 130 | 130 | 130 |
1) MD - Machine Direction - TD